SUNTACK
|
Apperance
|
Color
* 1
|
Bromine Value
|
Softeningpoint
* 2
|
Molecular Weight
* 3
|
Applications
|
|
U-90
|
Light yellow pellet
|
Max6
|
<25
|
100 5
|
1,000
|
A/F/R
|
|
U-101
|
Light yellow pellet
|
Max7
|
<25
|
110 5
|
1,000
|
A/C/F/R
|
|
U-120
|
Light yellow pellet
|
Max6
|
<25
|
120 5
|
1,000
|
A/C/F/P/R
|
|
U-140
|
Light yellow pellet
|
Max7
|
<25
|
140 5
|
1,000
|
A/C/F/P/R
|
|
|
|
GS-90
|
Amber pellet
|
Max9
|
<30
|
100 5
|
1,000
|
A/F/R
|
|
GA-100R
|
Amber pellet
|
Max12
|
<30
|
100 5
|
1,000
|
A/C/F/R
|
|
GA-100
|
Amber pellet
|
Max12
|
<30
|
105 5
|
1,000
|
A/C/F/R
|
|
|
|
SK-120
|
Amber pellet
|
Max8.5
|
<30
|
120 5
|
1,000
|
A/C/F/P/R
|
|
SK-120B
|
Amber pellet
|
Max11
|
<30
|
120 5
|
1,000
|
A/C/F/P/R
|
|
|
|
YT-130
|
Amber pellet
|
Max9
|
<30
|
130 5
|
1,200
|
A/C/P
|
|
YT-140
|
Amber pellet
|
Max9
|
<30
|
140 5
|
1,300
|
A/C/P
|
*
1. Color (Gardner)ASTM D -1154 :
50% in Toluene.
*
2. Ring & Ball Method ASTM - D 6493
*
3. Molecular weight measured by Vapor Pressure Osmometer Method.
|
Application :
|
A --> Adhesive
|
C --> Coating
|
F --> Floor Tiles
|
P --> Printing Ink
|
R --> Rubber
|
STORAGE
AND INVENTORY CONTROL
Pellet forms of low-to-medium softening point resins under the following
conditions may block, lump or fuce :
1.
During hot weather.
2. Upon prolonged storage.
3. If stored near any source of heat
|
|